Phone: +91 9818615900

Epichlorohydrin Rubber

  • Home
  • Epichlorohydrin Rubber

Epichlorohydrin Rubber

Our firm is affianced in offering an extensive range of Epichlorohydrin Rubber (ECO). Our product is made under the inspection of
knowledgeable experts using the advanced techniques and best grade material. Besides, this product can be availed in numerous
patterns as per the specific needs of our patrons.


Specification:

Brief introduction Epichlorohydrin rubber CO homopolymerized by epichlorohydrin, the molecular chain does not contain the double bond, the side chain is the chloromethyl, has the excellent oil resistance, heat resistance of aging, ozone resistance and gas resistance.
Molecular structure -(CH2-CH-O-)n-
                 ∣
                 CH2Cl
           
Technical data Grade? Mooney viscosity Cl content% Ash content% Water content% Density Ourward appearance
CO 3604 40±5 36~38 <1.0 <1.0 1.3±0.1 Light yellow to hazel
CO 3605 50±5
CO 3606 60±5
Commonly used materials Basic ingredients
(1)Vulcanization system:Oxide metallic/thioure、amines、
triazie、sulphur、peroxide
CO 100
(2)Reinforce Syste:Carbon black、Inorganic filling. StZn 1
NBC 1
(3)Anti-Aging System:Anti NBC,Anti MB Anti RD and ceresin wax etc. Pb3O4 5
Na-22 1.5
(4)Soften System:DOP TP-95 etc。 Carbon black N550 45
       
(5)Antiscorching agent:O-amino thiophenol etc. Physical Performance of Vulcanized Rubber
1、Normal feature? 170℃×20min? Secondary vulcanization 150℃×2hrs
Application  Hs(shoreA) 68
Tensile strength at break Tb (Mpa) 14.3
1、Various oil resistant rubber tube. Elongation at break
Eb (%)
460
2、Various diaphram. 2、Heat resistance of aging 150℃×72hrs
3、Rubber rollers for printing and industry use. Hs(shoreA) 1
4、Oil resistant mechanical seal. Change rate of tensile strength at break Tb (%) 6
5、O ring, sealing gasket, seal ring. Change rate of elongation at break Eb (%) -7.6
6、Special cable sheath.
7、Rubber spare parts for refrigerating machines. Volume change △V(%) 2.9
  5、Resistance to fuel C 40℃×48hrs
--
--- ---
-
Volume change △V (%) 40
6、Cold resistance
Bending fracture temperature T (℃) -25
Brief introduction Epichlorohydrin rubber ECO copolymerized by epichlorohydrin, ethylene oxide, the molecular chain does not contain the double bond, the side chain is the chloromethyl, has the excellent? oil resistance, heat resistance of aging, cold resistance and half electrical conductivity.
Molecular structure ?-(CH2-CH-O-)n-(CH2-CH2-O-)2-
                 ∣
                 CH2Cl
           
Technical data Grade? Mooney viscosity Cl content% Ash content% Water content% Density Ourward appearance
ECO 2404 40±5 24~27 <1.0 <1.0 1.20±0.1 Light yellow to hazel
ECO 2405 50±5
ECO 2406 60±5
Commonly used materials Basic ingredients
(1)Vulcanization system:Oxide metallic/thioure、amines、
triazie、sulphur、peroxide
ECO 100
(2)Reinforce Syste:Carbon black、Inorganic filling. StZn 1
NBC 1
(3)Anti-Aging System:Anti NBC,Anti MB Anti RD and ceresin wax etc. Pb3O4 5
Na-22 1.5
(4)Soften System:DOP TP-95 etc。 Carbon black N550 50
       
(5)Antiscorching agent:O-amino thiophenol etc. Physical Performance of Vulcanized Rubber
1、Normal feature? 170℃×20min? Secondary vulcanization 150℃×2hrs
Application Hs(shoreA) 71
Tensile strength at break Tb (Mpa) 13.5
1、Various oil resistant rubber tube. Elongation at break
Eb (%)
410
2、Various diaphram. 2、Heat resistance of aging 150℃×72hrs
3、Rubber rollers for printing and industry use. Hs(shoreA) -1
4、Oil resistant mechanical seal. Change rate of tensile strength at break Tb (%) -21
5、O ring, sealing gasket, seal ring. Change rate of elongation at break Eb (%) -43
6、Special cable sheath. 3、Compression set (%)
7、Rubber spare parts for refrigerating machines. 125℃×72hrs 30% 39
  4、Resistance to 903# oi 125℃×72hrs
Hs(shoreA) -1.5
Change rate of tensile strength at break Tb (%) -5.6
Change rate of elongation at break Eb (%) -21
Volume change △V (%) 3.1
5、Resistance to fuel C 40℃×48hrs
Volume change △V (%) 43
6、Cold resistance
Bending fracture temperature T (℃) -42
Brief introduction Hyperoxide epichloryhydrin rubber PECO copolymerized by epichlorohydrin, epoxy ethane and epoxy propane, the molecular chain does not contain double bond, the side chain contains chloromethyl, has the excellent features of ozone-resisting , with good cold resistance, elastic and half electrical conductivity.
Molecular structure -(CH2-CH-O-)n-(CH2-CH2-O-)m-(CH2-CH2-O-)2- CH3
                    ∣
                   CH2Cl
           
Technical data Grade? Mooney viscosity Cl content% Ash content% Water content% Density Ourward appearance
PECO 1204 40±5 12~18 <1.0 <1.0 1.20±0.1 Light yellow to hazel
PECO 1205 50±5
PECO 1206 60±5
Commonly used materials Basic ingredients
(1)Vulcanization system:Oxide metallic/thioure、amines、
triazie、sulphur、peroxide
PECO 100
(2)Reinforce Syste:Carbon black、Inorganic filling. StZn 1
NBC 1
(3)Anti-Aging System:Anti NBC,Anti MB Anti RD and ceresin wax etc. Pb3O4 5
Na-22 1.5
(4)Soften System:DOP TP-95 etc。 Carbon black N550 50
       
(5)Antiscorching agent:O-amino thiophenol etc. Physical Performance of Vulcanized Rubber
1、Normal feature? 170℃×20min? Secondary vulcanization 150℃×2hrs
Application  Hs(shoreA) 68
Tensile strength at break Tb (Mpa) 12.8
1、All kinds of damping rubber brick. Elongation at break
Eb (%)
430
2、Special diaphragm. 2、Heat resistance of aging 120℃×72hrs
3、Rubber rolls of office and industry. Hs(shoreA) 2
4、Oil resistant mechanical seal. Change rate of tensile strength at break Tb (%) -19
5、O ring, sealing gasket, seal ring. Change rate of elongation at break Eb (%) -26
  3、Compression set (%)
125℃×72hrs 30% 37
4、Resistance to 903# oi 125℃×72hrs
Hs(shoreA) -7
Change rate of tensile strength at break Tb (%) -8.6
Change rate of elongation at break Eb (%) -25
Volume change △V (%) 9.2
5、Resistance to fuel C 40℃×48hrs
Volume change △V (%) 65
6、Cold resistance
Bending fracture temperature T (℃) -55
Brief introduction Epichlorohydrin rubber GECO:Copolymerized by epichlorohydrin, epoxy ethane and allyl glycidyl ether, molecular chain contains double bond, the side chain contains chloromethyl, has the excellent features of ozone-resisting , resistant to soften the aging, cold resistance, and half electrical conductivity.
Molecular structure -(CH2-CH-O-)n-(CH2-CH2-O-)m-(CH2-CH2-O-)2-
                 ∣                                                                      ∣
                 CH2Cl                                                            CH2=CH-CH2-O-CH2
           
Technical data Grade? Mooney viscosity Cl content% Ash content% Water content% Density Ourward appearance
GECO 1204 40±5 12~18 <1.0 <1.0 1.20±0.1 Light yellow to hazel
GECO 1205 50±5
GECO 1206 60±5
Commonly used materials Basic ingredients
(1)Vulcanization system:Oxide metallic/thioure、amines、
triazie、sulphur、peroxide
ECO 100
(2)Reinforce Syste:Carbon black、Inorganic filling. StZn 1
NBC 1
(3)Anti-Aging System:Anti NBC,Anti MB Anti RD and ceresin wax etc. Pb3O4 5
Na-22 1.5
(4)Soften System:DOP TP-95 etc。 Carbon black N550 50
       
(5)Antiscorching agent:O-amino thiophenol etc. Physical Performance of Vulcanized Rubber
1、Normal feature? 170℃×20min? Secondary vulcanization 150℃×2hrs
Hs(shoreA) 69
Application Tensile strength at break Tb (Mpa) 13.1
1、Rubber covered roller of printer, duplicator. Elongation at break
Eb (%)
430
2、Various kinds of diaphragm. 2、Heat resistance of aging 120℃×72hrs
3、O ring, sealing gasket, seal ring. Hs(shoreA) 3
Change rate of tensile strength at break Tb (%) -18
Change rate of elongation at break Eb (%) -27
3、Compression set (%)
125℃×72hrs 30% 39
4、Resistance to 903# oi 125℃×72hrs
Hs(shoreA) -9
Change rate of tensile strength at break Tb (%) -10
Change rate of elongation at break Eb (%) -24
Volume change △V (%) 12
5、Resistance to fuel C 40℃×48hrs
Volume change △V (%) 66
6、Cold resistance
Bending fracture temperature T (℃) -55